After the first enthusiasm I managed to make my printer work a little sustained and the limit of some materials come up.
Unfortunately the only thing that make those bars not valid for be used in an enclosed environment is the Delrin. This is a good material for lots of application , it versatility lies in the good resistance at friction and the possibility to be cnc milled very good. BUT with the heat the game change.
With Haydn make we made this experiment and unfortunately it didn't succeeded.
After long print in an enclosed system with a temp of 60 Celsius (i meant 20+ hours at print) , despite using the proper lubricant changed at each print (super-lube), the Delrin start to consume making the magnet inside the bar come to touch the metal ball , finally scratching it.
I have several other ball sets so now the evolution of this project is substitute the Delrin with some metal ones. I have to ask to friends with good lathe.
I'll let you know how to the stuffs will go...